Kelas lan Komposisi Kimia (%)
| Kelas | C≤ | Si | Mn | P≤ | S≤ | Cr | Mo |
| SCM 420TK | 0.18~ 0.23 | 0.15~ 0.35 | 0.60~ 0.85 | 0.030 | 0.030 | 0.90~ 1.20 | - |
| SCM 415TK | 0.13~ 0.18 | 0.15~ 0.35 | 0.60~ 0.85 | 0.030 | 0.030 | 0.90~ 1.20 | 0.15~ 0.30 |
| SCM 418TK | 0.16~ 0.21 | 0.15~ 0.35 | 0.60~ 0.85 | 0.030 | 0.030 | 0.90~ 1.20 | 0.15~ 0.30 |
| SCM 420TK | 0.18~ 0.23 | 0.15~ 0.35 | 0.60~ 0.85 | 0.030 | 0.030 | 0.90~ 1.20 | 0.15~ 0.30 |
| SCM 430TK | 0.28~ 0.33 | 0.15~ 0.35 | 0.60~ 0.85 | 0.030 | 0.030 | 0.90~ 1.20 | 0.15~ 0.30 |
| SCM 435TK | 0.33~ 0.38 | 0.15~ 0.35 | 0.60~ 0.85 | 0.030 | 0.030 | 0.90~ 1.20 | 0.15~ 0.30 |
| SCM 440TK | 0.38~ 0.43 | 0.15~ 0.35 | 0.60~ 0.85 | 0.030 | 0.030 | 0.90~ 1.20 | 0.15~ 0.30 |
| Cathetan: 1. Ni minangka rereged ing macem-macem pipa baja ora ngluwihi 0,25%, lan Cu ora ngluwihi 0,30%;2. Nalika panuku njaluk analisis produk rampung, deviasi sing diidinake kaya sing ditemtokake ing Tabel 3 JIS G0321. | |||||||
Pabrik: pipa seamless (rampung panas lan rampung adhem)
Ukuran: OD: 15.0~114mm WT: 2~20mm
Kelas: SCM 415TK, SCM 420 TK.
Dawane: 6M utawa dawa sing ditemtokake kaya sing dibutuhake.
Ujung: Ujung Polos, Ujung Miring.
Kelas
Kode metode produksi (pipa baja seamless sing wis rampung panas: SH; Pipa baja seamless sing wis dirampungake adhem: SC)
Dimensi (diameter nominal X kekandelan tembok nominal utawa diameter njaba X kekandelan tembok)
Jeneng pabrikan utawa merek identifikasine
-
- Toleransi OD lan WT
Divisi
Toleransi ing OD
Toleransi ing WT
Kelas 1
D <50m
±0,5 mm
S <4mm
+0.6mm
-0.5mm
50mm≤D
±1%
S≥4mm
+1% -12,5%
Kelas 2
D <50m
±0.25mm
S <3mm
±0.3mm
50mm≤D
±0,5%
S≥3mm
±10%
Kelas 3
D <25m
±0,12 mm
S <2mm
±0.15mm
40mm>D≥25mm
±0,15 mm
50mm>D≥40mm
±0,18 mm
S≥2mm
±8%
60mm>D≥50mm
±0,20 mm
Cathetan: toleransi ing saben kekandelan tembok kudu dibulatke dadi siji desimal miturut aturan a JIS Z 8401
70mm>D≥60mm
±0.23mm
80mm>D≥70mm
±0,25 mm
90mm>D≥80mm
±0.30mm
100mm>D≥90mm
±0,40 mm
D≥100mm
±0,50%
1. Toleransi OD pipa baja seamless finish panas miturut Kelas 12. Pipa baja sing dipadamke lan ditemper miturut 4 kategori.
- Toleransi OD lan WT